Nevertheless, as soon as the SCPP was included with the scaffolds, the overall pH increased showing intrinsic task regarding the scaffold to buffer the SCPP. Additionally, mobile viability had been seen for as much as 21 times in scaffolds with early mineralization at 0.3, 0.5, and 1 mg/mL of SCPP. Overall, low amounts of SCPP proved to be a potential additive in biomaterial methods for bone tissue tissue engineering; nonetheless, the cytotoxic results because of it